  • The hardness of the sintered product of the present invention can be enhanced by adding preferably 0.01 to 0.50 mol %, relative to Al2O3, of metal oxide such as titanium oxide (TiO2 and the like), rare earth metal oxide (Y2O3, Yb2O3 and the like) and the like in the sintered product.