Then, by using a pulverizing means such as the mortar and the ball mill or the like, the fired matter is pulverized to obtain a prescribed average particle size, and the phosphor expressed by the composition formula SrAlSi6.5O1.25N9.50:Eu (wherein Eu/(Sr+Eu)=0.030) can be manufactured.