In a preferred procedure, the metal compound D) is initially taken, preferably in a solvent, such as heptane, the liquid alk-1-ene is added and the supported catalyst is added while stirring at from 0 to 100??? C. The polymerization time may be from 0.01 to 24, preferably from 0.1 to 5, hours.