As previously stated, the polyester polyols of the present invention are preferably prepared by polycondensation under azeotropic conditions or most preferably in the melt, catalyst free or preferably while using transesterification catalysts, in an atmosphere of an inert gas such as nitrogen, carbon monoxide, helium, argon, and the like, at temperatures from 80??? to 250??? C., preferably from 15