For example, the opening depth may range from about 1 micron to about 5 microns in typical contact or bonding pads. [0029] Still referring to FIG. 1D, following electrodeposition of copper layer 24A, in one embodiment of the present invention, a second barrier layer 20B including the preferred embodiments detailed for the first barrier layer 20A is formed over copper layer 24A followed by formatio