A self-supporting thermoplastic polymer film characterized in that said film is a heat-tempered film having reduced core-set curling tendency and that the change in ANSI curl units that said film undergoes upon being maintained in rolled condition for 2200 hours at a temperature of 21??? C. and R.H. up to 50% is at least 15% less than the change in the number of ANSI curl units that the correspond