For example, if the thin film is a metal film, such as a copper film, the etchant can include a mixture of hydrofluoric acid and hydrogen peroxide, as an oxidizing agent, most preferably 0.5% hydrofluoric acid and 10% hydrogen peroxide, by volume, with the remainder being deionized water.