Typically, the rubbers, such as a styrene-butadiene rubber and polybutadiene are mixed in a first stage with various fillers such as the extra conductive carbon black, the silica and the various processing aids and antioxidants for about 6 minutes or until a Banbury thermocouple reaches about 320??? F., whichever occurs first.