In order to achieve a satisfactory reduction of the contact resistance however with a material expense which is as low as possible, the coating in the case of a coating with graphite is preferably to be carried out with a layer thickness of between 5 ??m and 200 ??m, particularly preferably between 10 ??m and 100 ??m.