The isolation of the composite comprising the solid carrier and, adsorbed thereon, the particles protected by the protective polymer is performed for example, by separating the composite from the dispersion medium, washing the separated composite with a solvent, such as water or an alcohol, and drying the washed composite at 10??? to 80??? C., preferably at 20??? to 30??? C. under vacuum.