This process provides substrates W that have a plated film 504 grown in the opening 502 a formed in the resist 502, as shown in FIG. 27B. The substrate W which has been spin dried, as described above, is immersed in a solvent, such as acetone, that is maintained at a temperature of 50-60??? C., for example.