Then, as shown in FIG. 7 d, a non-magnetic layer 41 of an insulating material such as Al2O3, SiO2, AlN or DLC or a metal material such as Ti, Ta or Pt with a thickness of approximately 0.1-0.5 ??m is formed to isolate the MR effect element 33 from an electromagnetic coil element which will be formed later.