According to this method, even if a thin oxide film (at a thickness of, for example, 10 to 20 ???) or contaminant such as carbon derived from a vacuum pumping system remains on the surface of the silicon wafer before the metal is deposited, the stable metal silicide layer is easily formed by reacting the metal and the silicon.