It is possible to perform within a single sputter reactor a two-step copper PVD process in which the first step produces the structure of FIG. 19 and the second step is performed with chamber parameters adjusted to reduce the copper ion energy so that, as illustrated in the cross-sectional view of FIG. 20, the via bottom is coated with a second copper layer 292 covering all areas including a via b