It is also preferred that the temperature difference between the MD of the second component and the foaming treatment temperature is 20??? C. or greater, more preferably 50??? C. or greater, especially 80??? C. or greater, in order to minimize reduction of the degree of orientation of the second component, i.e, any reduction in the strength, caused by the heat applied during the foaming treatment.