t temperatures of from about 25??? to 250??? C., more preferably 70??? to 180??? C. Depending upon whether the hydrocarbon to be oxidized is a solid, liquid, or gas, it is dissolved in or bubbled through the solvent, together with air or oxygen, in the presence of the aforementioned nitride-activated metal coordination complex catalyst for periods of time sufficient to yield the desired oxidized p