The halogen treatment, for example, chlorine treatment of the catalyst can be accomplished by exposing the catalyst in either dry or slurry form to gaseous chlorine at 1.0 to 10 atmospheres total pressure for about 10 minutes to 4 hours at temperatures ranging from about 0??? to 100??? C. A mixture of Cl2 and an inert gas such as argon or nitrogen can also be employed.