The solid phase polymerization may be performed using a resin composition formed into a chip, powder, fiber, plate or block shape, at a temperature of from 170 to 220??? C. for approximately from 3 to 48 hours in the presence of an inert gas such as nitrogen or argon or under reduced pressure of 100 torr or less, preferably 10 torr or less.