| - Further, when a phosphor is fired in O2, O2???N2, or O3???N2, degradation characteristics of the phosphor can be inhibited by coating it with materials, such as Al2O3, SiO2, ALF3, La2O3, and LaF2, by hydrolysis using metal alkoxide or acetylacetone, at the same time
|