After the rough socket forging 42 is formed by the progressive hot-forging steps or operations, the rough forging 42 is normalized by heating the forging to a temperature of approximately 1,650 degrees F. After the rough forging 42 cools, it is lubricated by dipping the forging in a material such as borax.