After the porous Li(Mg0.05Co0.95)O2 structure is sintered at 900-1150??? C. in air or oxygen, it is cooled in an inert atmosphere such as nitrogen or argon, during which process the exposed outer surface of the cathode away from the current collector is more reduced than the interior section adjacent to the current collector.