A method as in claim 2, wherein the step of introducing comprises operating a growth chamber at a moderate substrate temperature while providing the anion atoms, cation atoms and the dopant atoms, and while maintaining a low background pressure for oxygen atoms, radicals, molecules and oxygen-containing or bearing compounds and other contaminating materials. 4.