The wafers are then be positioned and sealed in the deposition chamber, whereupon heating elements bring the temperature of the chamber to about 640??? C. to 800??? C. Utilizing a pump, the system is then pumped down to a pressure of about 10 mTorr or less after which the deposition chamber is purged using N2 or other inert gas.