To produce the BG, compounds such as calcium nitrate, triethyl phosphate and tetraethyl orthosilicate were used as precursors and hydrolyzed to form a sol???gel solution, which was then added to a polyacrylonitrile (PAN) solution in N,N-dimethylformamide.