As shown in FIG. 5, further, each infiltrated body 6 was placed on a refractory plate 3 so that both sides thereof were held and supported by alumina bars 4, and heated to 1150??? C. in a hydrogen atmosphere, thereby re-melting and solidifying the components mainly composed of copper.