It was then impregnated with chromium as in the previous examples (0.5 weight percent Cr) and oxidized in air for 1 hour at 316??? C. Polymerization runs were carried out as before at 102??? C. This is invention Run A. In run B, the same procedure was followed except no I2 was used.