In this case, a line width of the second conductive film 104 is 5 to 10 ??M. In the etching, dry etching with gas including chlorine is performed providing pressure inside an etching treatment chamber is reduced (including vacuum) and heating or irradiation of light is performed to a surface of the substrate.