Then the solution is spread on a surface such as a glass plate or cloth preferably at a predetermined temperature in the range of 10??? to 85??? C, with a doctor blade or an applicator to form a film a thickness of 0.1 to 0.30 mm, preferably 0.15 to 0.25 mm.