| - For example, in the so-called solvent polymerization where an inert diluent is used, a hydrocarbon solvent such as hexane, heptane, cyclohexane, benzene, toluene, xylene, etc. can be used, and it is commonly practiced at a polymerization temperature ranging from 0??? C. to 120??? C., preferably from 20??? C. to 90??? C. The polymerization pressure is also widely variable.
|