Once the two- or multilayer extrudate has been extruded and ???wound??? onto the former of diameter d, it is sintered on the former in a furnace at a temperature in the region of 900-1,000??? C. Surface electrodes can then be added to any external active layers by, for example, the sputtering of a conductive material such as silver or aluminum.