Subsequently, some of the samples (Al-12w%Si/50v%SiCp) were tested to determine physical properties such as thermal conductivity and CTE. The test results revealed that they had 124 W/(m-K) thermal conductivity, point A in FIG. 6 and 10.8 ppm/K CTE, point A in FIG. 7.