In the preferred embodiments of the invention, the amount of nucleating agent employed is in the range of from about 0.15 to about 1 weight percent based on the total weight of polyolefin and agent, and in the particularly preferred embodiments of the invention is from about 0.2 to about 0.6 weight percent on the aforementioned basis.