In Formula 4, a, b, c and d are either hydrogen or alkyl group of 1-4 carbon atoms or combination of hydrogen and alkyl or other functional groups such as carboxyl or halogen, extruding the mixture at a temperature between 170-210??C to obtain the semi crystalline thermoplastic polymer having improved crystallization temperature (Tc) and reduced spherulitic size and hence improved transparency cha