In another embodiment, the medical wire is heated to a temperature, depending on the metal alloy or other material of the medical wire, in excess of at least 700?? F. (371?? C.) for a period of time sufficient to thermally degrade surface impurities, draw oils and other impurities out of any pores in the surface of the medical wire and create a non-acidic ???passivation??? of the surface of the me