The resulting silicon oxide layer preferably has a thickness of about 0.6 to about 1.5 nanometers and a concentration of no more than 1???109 atoms/cm2, more preferably no more than about 1???103 atoms/cm2 of each of iron, chromium, titanium and other metals which degrade minority carrier lifetime.