Thus, once again this portion of heat sealed area 118 between the release layer 102 and the membrane 130 is peelable by virtue of the presence of release coating 104 therebetween, sand its effect upon weakening of the thermal bond produced therebetween or by use of other methods for achieving this result, such as the use of differing thermoplastic layers as is discussed above, In any event, the th