The bottom electrode 20 heats the semiconductor substrate to a temperature from about 100??? C. to about 350??? C., and preferably from about 200??? C. to about 300??? C. A gaseous material 30 including a reducing agent such as ammonia is directed to manifold 14 from one or more gas lines 12.