As a sample of the present invention, a sintered body 7 of the Cu--W alloy prepared in the aforementioned manner was stood vertically upright on a refractory plate 3 and both sides thereof were held and supported by alumina bars 4 as shown in FIG. 6, and heated to 1200??? C. in a hydrogen atmosphere again, thereby re-melting and solidifying the components mainly composed of copper.