The photoinitiator is generally added at about 0.5 to 4 phr (part per hundred resin) to the resin composition having acrylate functionality, resulting in about 0.5 wt % to about 3.0 wt % photoinitiator in the hard coat composition, depending on the amount of solvent and other additives discussed below.