ng material, then an oxygen absorbent mainly composed of iron and having an oxygen absorbing capacity of 600 ml was disposed therebetween, and the joined sheet and packaging material were heat sealed edgewise by heating under pressure at 130??? C. for 3 seconds so as to encapsulate the oxygen absorbent.