rom about 12 hours to about 1 week, and preferably about 24 hours, with a solvent, such as N,N-dimethylformamide, to provide Type V hydroxygallium phthalocyanine having excellent xerographic characteristics when selected as a photogenerator in a layered photoconductive imaging member with a supporting substrate and a charge transport layer.