The structure of FIG. 50 is similar to that of FIG. 49 except that the fourth-layer interconnection 13L (BP) is formed of the thick conductor film 13L2 made of an Al base material and the thin conductor film 13L1 formed from a high-melting point metal or metal compound such as TiN or W. This structure brings about a further improvement in the reliability.