The method according to claim 2, wherein the polyolefin resin is a mixture consisting of from 30 to 90% by weight of a low-density polyethylene having a density of not more than 0.930 g/cc and 70 to 10% by weight of a high-density polyethylene having a density of not less than 0.940 g/cc.